When using a constant Thermostatic Waterbath or some other experimental equipment, the inner tank, outer casing or some metal parts are prone to rust. Since the serious rust will affect the performance of the equipment and directly affect the experimental results, what can we do when we use it? Or put an end to rusting equipment?
1 Since the outer casing is made of electrostatic spray technology, it can effectively prevent rust under normal conditions, but in a highly corrosive environment, the effect will be weakened, so we recommend that all Stainless Steel Thermostatic Waterbath be used in this type of environment.
2 In the sink, we use the all-stainless steel of the electronic universal testing machine. In this case, the rusting ability will be weakened, but the stainless steel is not rusting, but it is more resistant to corrosion than ordinary metals, so we finished the experiment. After that, drain the working water in the sink and dry it in the air.
3 people's sweat will also cause the equipment to rust, sweating is inevitable, to avoid rust caused by hand sweat, production personnel or experimenters should bring gloves, finger cots, or use special tools to take parts, do not use Hand touch the product.
4 Let me talk about the simple method of applying anti-rust oil:
1. Soaking method: 1 small items should be immersed in anti-rust grease, so that the surface is adhered with a layer of anti-rust grease. The oil film thickness can be reached by controlling the temperature or viscosity of the rust preventive grease.
2. The brushing method is used for outdoor building equipment or special-shaped products that are not suitable for soaking or spraying. When brushing, it is necessary to pay attention not to accumulate, and also to avoid leakage coating.